-- Select Area --
Description
| COMPOSITION | PVC - 78%, PU - 2% & Polyester |
|---|---|
| WEIGHT | 1000 grams per linear meter ±5% |
| WIDTH | 137 cms / 54 inches ±2% |
| ABRASION | In excess of 1,00,000 cycles Martindale Abrasion Tester at 12 kPa pressure |
| WYZENBEEK ABRASION | ASTM D4157 - 1,50,000 (#10 cotton duck) |
| BALLY FLEXING TEST | @-10 - SATRA - PM 55 - 1.5 LAC |
| FLEXING TEST | As per SATRA - TM 55:1999 |
| FLAMMABILITY | BS EN 1021-1:1994 (Cigarette Test); Pass BS EN 1021-2:1994 (Match Flame Test); Pass CAL-117 (Cigarette Test, Annexure B) Note: Flammability performance is dependent on the combination of material used |
| PASSING BIS METHOD | IS 15768: 2008 (RA-2018) IS 12467: Part-1: 2006 & IS 12467: Part-2: 2006 |
| SOIL RELEASE | AATCC 130-2018 |
| ANTIMICROBIAL | AATCC-100 |
| MAINTENANCE | Do not use abrasive cleaner |
| FASTNESS TO LIGHT | Above 5; ISO 105-B02: 2014 |
| FASTNESS TO RUBBING | Dry: 4.5; & Wet: 4; ISO-X12:2016 |
| USAGE | Upholstery, sofas, chair, acoustic recliners, auditorium seatings, modular furniture |
| COLOUR MATCHING | Batch to batch variation in shade may occur within commercial tolerances |